==Roughness of thermally evaporated aluminium==
==Roughness of thermally evaporated aluminium==


A study by AFM was performed to examine the Al films deposited with thermal evaporation in the Wordentec. See details of the study [[/Comparison of roughness and other surface characteristics for different methods of Aluminium deposition|here]].
A study by AFM was performed to examine Al films deposited with thermal evaporation in the Wordentec. See details [[/Roughness of thermally evaporated aluminium|here]]. [[/Comparison of roughness and other surface characteristics for different methods of Aluminium deposition|here]].