Descum results
Plasma asher 1
Descum of AZ5214E resist on 50mm silicon wafer. Wafer was placed horisontally in chamber on a 100 mm carier wafer.
Note: Plasma asher was cold before use
|
Conny Hjort & Jesper Hanberg September 2019
Plasma asher 2
Descum of AZ Mir 701 resist on 100mm silicon wafer. Five wafers were placed vertically in chamber.
Experiment parameters:
|
recipe 1
|
recipe 2
|
We can observe linear dependance of etched material on time after etching 7 minutes and more (recipe 2).