Topas polymers are supplied by Nanolab. All other polymers are purchased by the users themselves. All polymers (and each individual grade of each polymer) must be approved for use at DTU Danchip. If you would like to use a new polymer or a new grade of a certain polymer, please fill out the application form which can be found in LabManager by going to the 'Documents' tab of the 'Info' page for the Polymer Injection Molding machine. You can also click this direct link: [http://labmanager.dtu.dk/view_binary.php?fileId=2857 New_polymer_application.dotx]. | Topas polymers are supplied by Nanolab. All other polymers are purchased by the users themselves. All polymers (and each individual grade of each polymer) must be approved for use at DTU Danchip. If you would like to use a new polymer or a new grade of a certain polymer, please fill out the application form which can be found in LabManager by going to the 'Documents' tab of the 'Info' page for the Polymer Injection Molding machine. You can also click this direct link: [http://labmanager.dtu.dk/view_binary.php?fileId=2857 New_polymer_application.dotx]. | ||
When the polymer has been approved you will receive labels which must be used to label your polymer. All polymers left in the injection molding room must be marked with this official DTU | When the polymer has been approved you will receive labels which must be used to label your polymer. All polymers left in the injection molding room must be marked with this official DTU Nanolab label. '''Polymers not labelled appropriately may be thrown out at any time'''. | ||
The easiest way to get an overview of polymers and processes used on the polymer injection molding machine is to go to LabManager and consult the [http://labmanager.dtu.dk/function.php?module=Processlog&view=editlog&machid=278 Process Log for the injection molding machine]. If you would like use a non-Nanolab polymer for a test, please contact the owner of the polymer and ask if you can have a sample. A complete list of all polymers in use at DTU Nanolab and who owns them can be found in LabManager on the Info page for the polymer injection molding machine on the 'Documents' tab. You can also click this direct link: [http://labmanager.dtu.dk/view_binary.php?fileId=3044 Approved_polymers_list.pdf]. | The easiest way to get an overview of polymers and processes used on the polymer injection molding machine is to go to LabManager and consult the [http://labmanager.dtu.dk/function.php?module=Processlog&view=editlog&machid=278 Process Log for the injection molding machine]. If you would like use a non-Nanolab polymer for a test, please contact the owner of the polymer and ask if you can have a sample. A complete list of all polymers in use at DTU Nanolab and who owns them can be found in LabManager on the Info page for the polymer injection molding machine on the 'Documents' tab. You can also click this direct link: [http://labmanager.dtu.dk/view_binary.php?fileId=3044 Approved_polymers_list.pdf]. | ||