Specific Process Knowledge/Thin film deposition/Deposition of Aluminium: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 64: | Line 64: | ||
Studies by AFM was performed to examine differences in characteristics of the Al films, deposited with the differnt methods (sputter, e-beam, thermal). See details of the study [[/Comparison of roughness and other surface characteristics for different methods of Aluminium deposition|here]]. | Studies by AFM was performed to examine differences in characteristics of the Al films, deposited with the differnt methods (sputter, e-beam, thermal). See details of the study [[/Comparison of roughness and other surface characteristics for different methods of Aluminium deposition|here]]. | ||
==Aluminium deposition on AZ5214 for lift-off== | |||