==PhotoLuminescense Mapper RPM2000 == | ==PhotoLuminescense Mapper RPM2000 == | ||
| Line 12: | Line 12: | ||
'''The user manual and contact information can be found in LabManager:''' | '''The user manual and contact information can be found in LabManager:''' | ||
[http://www.labmanager | [http://www.labmanager.dtu.dk/function.php?module=Machine&view=view&mach=152 PL mapper] | ||
{| border="2" cellspacing="0" cellpadding="10" | {| border="2" cellspacing="0" cellpadding="10" | ||
| Line 62: | Line 62: | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*Software (free) to view and re-analyse the maps and spectra can be found on Labmanager. | *Software (free) to view and re-analyse the maps and spectra can be found on Labmanager. | ||
*Direct link to file download [http://labmanager | *Direct link to file download [http://labmanager.dtu.dk/view_binary.php?fileId=832 RPM2000 analysis software]. | ||
*The software will request you to get a (free) license key from Nanometrics. | *The software will request you to get a (free) license key from Nanometrics. | ||
|} | |} | ||