Jump to content

Specific Process Knowledge/Characterization/Four-Point Probe: Difference between revisions

Paphol (talk | contribs)
Paphol (talk | contribs)
Line 6: Line 6:


The Four point probe is manufactured by Jandel Engineering Limited and using Jandel probe head and the RM3000+ Test Unit which can supply constant current between 10nA and 99.99mA, and measure voltage from 0.01mV to 1250mV.
The Four point probe is manufactured by Jandel Engineering Limited and using Jandel probe head and the RM3000+ Test Unit which can supply constant current between 10nA and 99.99mA, and measure voltage from 0.01mV to 1250mV.
For sheet resistance measurements, the quoted range is 1 milliohm/square to 5x108 ohms/square. Measurements outside this range are possible but with possible reduced accuracy. For volume (bulk) resistivity measurements, the quoted range is 1 milliohm.cm to 1x106 ohm.cm. Measurements outside of this range may be possible but will depend on sample type e.g. whether the sample is a thin layer.
For sheet resistance measurements, the quoted range is 1 milliohm/square to 5x108 ohms/square. Measurements outside this range are possible but with possible reduced accuracy. For volume (bulk) resistivity measurements, the quoted range is 1 milliohm.cm to 1x106 ohm.cm. Measurements outside of this range may be possible but will depend on sample type e.g. whether the sample is a thin layer. [[Image:Jandel_four_point_probe.PNG |thumb|600x600px|Four point probe: positioned in cleanroom D-3]]
Multiposition Probe stand can measure on wafers up to 200mm diameter. The Θ movement clicks in four positions at 90 degrees and the linear movement in up to 10 positions giving repeat placement accuracy of +/- 1mm.
Multiposition Probe stand can measure on wafers up to 200mm diameter. The Θ movement clicks in four positions at 90 degrees and the linear movement in up to 10 positions giving repeat placement accuracy of +/- 1mm.
    
    
The Four-Point Probe is a Veeco FPP-5000 for I/V measurement. The main purpose is to measure resistance and resistivity on a 4" silicon wafer. But can also be used to find thickness of thin layers or test if is a N- or P-type wafer.  
The Four-Point Probe is a Veeco FPP-5000 for I/V measurement. The main purpose is to measure resistance and resistivity on a 4" silicon wafer. But can also be used to find thickness of thin layers or test if is a N- or P-type wafer.  


The wafer are pushed down on the four pins so a measurement is performed. It works only for 4" wafers because a special holder is need.   
The wafer are pushed down on the four pins so a measurement is performed. It works only for 4" wafers because a special holder is need.   
[[Image:4pointprobe.jpg|thumb|300x300px|Four point probe: positioned in cleanroom D-3]]
[[Image:4pointprobe.jpg|thumb|300x300px|Four point probe: positioned in 346-904]]


'''The user manual, technical information and contact information can be found in LabManager:'''
'''The user manual, technical information and contact information can be found in LabManager:'''