Specific Process Knowledge/Thin film deposition/Deposition of AZO: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 2: | Line 2: | ||
AZO can be deposited by Sputtering process | AZO can be deposited by Sputtering process ad atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment. | ||
Revision as of 13:21, 10 July 2019
Feedback to this page: click here
AZO can be deposited by Sputtering process ad atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment.
| Sputtering deposition (Lesker) | Atomic layer deposition (ALD Picosun R200) | |
|---|---|---|
| General description | Sputter deposition of AZO | Atomic layer deposition of AZO |
| Pre-clean | RF Ar clean | |
| Layer thickness | 10Å to 5000Å* | 0 to 1000 Å |
| Deposition rate | Depending on process parameters. | Depending on temperature |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment |
|
* For thicknesses above 200 nm permission is required.