Specific Process Knowledge/Wafer cleaning/RCA: Difference between revisions
Appearance
| Line 6: | Line 6: | ||
The RCA cleaning procedure was originally developed by the Radio Corporation of America (RCA) as part of manufacturing electron tube components. This process has since been adapted to silicon semiconductor processing. RCA is a two-step process (RCA1 and RCA2, sometimes referred to as SC-1 and SC-2 (Standard Clean)), and RCA1 should always be made before RCA2 because removing organic contaminants is a requirement before metal contaminants can be removed effectively.<br> | The RCA cleaning procedure was originally developed by the Radio Corporation of America (RCA) as part of manufacturing electron tube components. This process has since been adapted to silicon semiconductor processing. RCA is a two-step process (RCA1 and RCA2, sometimes referred to as SC-1 and SC-2 (Standard Clean)), and RCA1 should always be made before RCA2 because removing organic contaminants is a requirement before metal contaminants can be removed effectively.<br> | ||
RCA1 is a powerful oxidizer and will thus remove organic contaminants. The ammonium hydroxide in RCA1 also has good solvating power as it can complex metals such as Cu, Ag, Ni, Co and Cd into solution. RCA2 forms soluble complexes with heavy metals and also shows cleaning action similar to that of piranha solutions. Furthermore, solutions of hydrochloric acid, which is a major constituent of RCA2, has proven effective at removing alkali metal ions. RCA2 is effective at removing metal hydroxide traces that cannot be removed in ammonia-containing solutions such as RCA1. These include Al(OH)<sub>3</sub>, Fe(OH)<sub>3</sub>, Mg(OH)<sub>2</sub> and Zn(OH)<sub>2</sub>. It is important that the chemicals used are very clean. RCA mixtures are therefore only used shortly after mixing and for a limited number of samples.<br> | RCA1 is a powerful oxidizer and will thus remove organic contaminants. The ammonium hydroxide in RCA1 also has good solvating power as it can complex metals such as Cu, Ag, Ni, Co and Cd into solution. RCA2 forms soluble complexes with heavy metals and also shows cleaning action similar to that of piranha solutions. Furthermore, solutions of hydrochloric acid, which is a major constituent of RCA2, has proven effective at removing alkali metal ions. RCA2 is also effective at removing metal hydroxide traces that cannot be removed in ammonia-containing solutions such as RCA1. These include Al(OH)<sub>3</sub>, Fe(OH)<sub>3</sub>, Mg(OH)<sub>2</sub> and Zn(OH)<sub>2</sub>. It is important that the chemicals used are very clean. RCA mixtures are therefore only used shortly after mixing and for a limited number of samples.<br> | ||
Since RCA1 can oxidize silicon to silicon dioxide, an HF dip is sometimes used between RCA1 and RCA2. This will also remove contaminants that can be trapped in the formed oxide. This step can also be omitted, since RCA1 removes the native oxide and then re-oxidizes the surface. This in itself has a cleaning action. It is generally not advised to do an HF dip after RCA-2 if the samples will be processed by wet chemical processes afterwards. This is because the hydrogenated surface will be extremely reactive and therefore attract contaminants from both the air and processing liquids. In this case it is better to continue processing with the passivated oxide surface. For furnace processes, an HF dip after RCA-2 makes more sense (but ideally the wafers should be transferred to the furnace processes immediately).<br> | Since RCA1 can oxidize silicon to silicon dioxide, an HF dip is sometimes used between RCA1 and RCA2. This will also remove contaminants that can be trapped in the formed oxide. This step can also be omitted, since RCA1 removes the native oxide and then re-oxidizes the surface. This in itself has a cleaning action. It is generally not advised to do an HF dip after RCA-2 if the samples will be processed by wet chemical processes afterwards. This is because the hydrogenated surface will be extremely reactive and therefore attract contaminants from both the air and processing liquids. In this case it is better to continue processing with the passivated oxide surface. For furnace processes, an HF dip after RCA-2 makes more sense (but ideally the wafers should be transferred to the furnace processes immediately).<br> | ||