*Speed vs. design
*Speed vs. design


Design: 5 100µm wide, 40mm long lines, spaced 10mm apart (40x40mm<sup>2</sup>)
{| cellpadding="2" style="border: 2px solid darkgray;" align="right"
! width="350" |
! width="350" |
|- border="0" align="center"
|[[Image:Labspin_2.JPG|300px]]
|[[Image:Labspin_3_+_fumehood_11.JPG|300px]]
|- align="center"
| This design printed in 6 minutes ||  This design printed in 1 minute
|}


<br clear="all" />
<br clear="all" />