Specific Process Knowledge/Lithography/Aligners/Aligner: Maskless 02 processing: Difference between revisions
Appearance
| Line 145: | Line 145: | ||
[[Image:MLA150_label.JPG|400x400px|thumb|An example of wafer ID produced by the labeling function]] | [[Image:MLA150_label.JPG|400x400px|thumb|An example of wafer ID produced by the labeling function]] | ||
The conversion manager software allows for inclusion of labels during the design conversion process. The labels are configured in a .lbl tab-delimited ASCII file with a special header in the first row, which must be located in HIMT\Designs\Labels folder. When used, the labels defined in the label file will be merged with the pattern in the source file, and the result can be inspected in the viewer. The X and Y positions of the labels should be given in design coordinates, and will be subject to any offsets/shifts applied to the design. | The conversion manager software allows for inclusion of labels during the design conversion process. The labels are configured in a .lbl tab-delimited ASCII file with a special header in the first row, which must be located in HIMT\Designs\Labels folder. When used, the labels defined in the label file will be merged with the pattern in the source file, and the result can be inspected in the viewer. The X and Y positions of the labels should be given in design coordinates, and will be subject to any offsets/shifts applied to the design. Note, that if the label file is changed, the job file will not update automatically. | ||
'''Example of a label file:''' | '''Example of a label file:''' | ||