According to specs, the writing speed of Aligner: Maskless 02 is 285mm<sup>2</sup>/min in fast mode. Using the high quality exposure mode cuts this speed in half, to approximately 140mm<sup>2</sup>/min. The writing speed for a 100x100mm<sup>2</sup> area measured during installation of the machine (acceptance test) was | According to specs, the writing speed of Aligner: Maskless 02 is 285mm<sup>2</sup>/min in fast mode. Using the high quality exposure mode cuts this speed in half, to approximately 140mm<sup>2</sup>/min. The writing speed for a 100x100mm<sup>2</sup> area measured during installation of the machine (acceptance test) was ~340mm<sup>2</sup>/min for both exposure wavelengths. | ||