Specific Process Knowledge/Lithography/Aligners/Aligner: Maskless 02 processing: Difference between revisions
Appearance
| Line 158: | Line 158: | ||
|-style="background:silver; color:black" | |-style="background:silver; color:black" | ||
| | | | ||
! | !Large | ||
! | !XLarge | ||
|- | |- | ||
|- | |- | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
! | !Intensity measurements | ||
| | |3.3 | ||
| | |17.4 | ||
|- | |- | ||
|- | |- | ||
|-style="background:LightGrey; color:black" | |-style="background:LightGrey; color:black" | ||
! | !150µm SU-8 dose tests | ||
|~3 | |||
|~10 | |||
| | |||
| | |||
|- | |- | ||
|- | |- | ||
|-style="background:LightGrey; color:black" | |-style="background:LightGrey; color:black" | ||
!AZ | !1.5µm AZ MiR 701 dose tests | ||
| | |7.5 | ||
| | |20.8 | ||
|- | |- | ||
|- | |- | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
! | !10µm AZ 4562 dose tests | ||
| | |? | ||
| | |? | ||
|- | |- | ||
|} | |} | ||