Specific Process Knowledge/Etch/Etching of Chromium: Difference between revisions
Appearance
| Line 34: | Line 34: | ||
!Etch rate range | !Etch rate range | ||
| | | | ||
*~ | *~150nm/min at room temperature | ||
| | | | ||
*~14 nm/min (depending on features size and etch load) | *~14 nm/min (depending on features size and etch load) | ||
Revision as of 13:49, 7 February 2019
Feedback to this page: click here
Etching of Chromium
Etching of chromium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Chromium Etch Methods
| Cr wet etch | ICP metal | IBE (Ionfab300+) | |
|---|---|---|---|
| Generel description | Wet etch of Cr premixed (Chrome etch 18) | Dry plasma etch of Cr | Sputtering of Cr - pure physical etch |
| Etch rate range |
|
|
|
| Etch profile |
|
|
|
| Substrate size |
|
|
Smaller pieces glued to carrier wafer
|
| Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
|
|