!SECTION UNDER CONSTRUCTION! | !SECTION UNDER CONSTRUCTION! | ||
AZ 5214E 1:1 by volume in PGMEA | Spin coating of AZ 5206E (AZ 5214E 1:1 by volume in PGMEA) dispensed from syringe on Spin Coater: Gamma UV is divided into two steps: Spin coating, and soft baking. The spin coating uses dynamic dispense of resist at 300 rpm, using a volume of 1.5 ml for 100 mm substrates. The dispense is followed by spin-off at a thickness dependent spin speed for 30 seconds with backside rinse. The wafer dried at 800 rpm for 15s before stopping. Soft baking is done at 90°C in 1 mm proximity for a thickness dependent time. The coating may be affected by the backside rinse at the very edge of the wafer, something which should be considered if the resist is used as an etch mask. | ||
''Sequence names, process parameters, and test results (Sequence no. 4000-4999):'' | ''Sequence names, process parameters, and test results (Sequence no. 4000-4999):'' | ||
*'''( | *'''(4405) 100mm 5206E 0,5um HMDS''' | ||
Spin-off: | Spin-off: ???? rpm. Soft bake: 60s? | ||
{|border="1" cellspacing="0" cellpadding="3" style="text-align:left;" | {|border="1" cellspacing="0" cellpadding="3" style="text-align:left;" | ||