*There are fewer particles from just loading/pumping/venting/unloading wafers with no processing in the Wordentec than the Temescal, at least when tested in Nov/Dec 2018.  
*There are fewer particles from just loading/pumping/venting/unloading wafers with no processing in the Wordentec than the Temescal, at least when tested in Nov/Dec 2018.  


The full results of the testing can be found here: .
The full results of the testing can be found here: [[:File:particles-pinholes test Temescal.pptx]].