== The Ti2p peak ==
== The Ti2p peak ==
The titanium Ti2p peak is notoriously difficult to fit. Let us first look for some clues in [[Specific Process Knowledge/Characterization/XPS/Processing/XPSknowledgeview |XPS Knowledge view]].
The titanium Ti2p peak is notoriously difficult to fit. Let us first look for some clues in [[Specific Process Knowledge/Characterization/XPS/Processing/XPSknowledgeview |XPS Knowledge view]]. The section below is a copy of the content in XPS Knowledge View (Avantage version 5.986).


=== XPS Knowledge on the fitting of the Ti2p peak ===
=== XPS Knowledge on the fitting of the Ti2p peak ===