Jump to content

Specific Process Knowledge/Back-end processing/Polisher CMP: Difference between revisions

From LabAdviser
Rkch (talk | contribs)
Rkch (talk | contribs)
Line 16: Line 16:
<!-- give the link to the equipment info page in LabManager: -->
<!-- give the link to the equipment info page in LabManager: -->
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=430 The Logitech Orbis (CMP) in LabManager]
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=430 The Logitech Orbis (CMP) in LabManager]


==Equipment performance and process related parameters==
==Equipment performance and process related parameters==

Revision as of 11:38, 29 November 2018

Feedback to this page: click here



Polisher (CMP)

The Logitech PM5 Polisher/Lapper

The Logitech Orbis Polisher (CMP) is for polishing wafers (removing material in the nm range) it is not for thinning down wafers or other substrates.


The user manual, user APV, technical information and contact information can be found in LabManager:

The Logitech Orbis (CMP) in LabManager

Equipment performance and process related parameters

Equipment Polisher/Lapper
Purpose

Polishing of

  • Silicon
  • SiO2
Performance 20x20mm substrate
  • Removal rate: 400nm/min
  • Thickness accuracy: +/- ? µm
  • Thickness homogeneity: +/- ? µm
  • Roughness: +/- ? µm
100mm substrate
  • Removal rate: ~ 60 nm/min
  • Thickness accuracy: ? µm
  • Thickness homogeneity: ? µm
  • Roughness: +/- ? µm
Process parameter range Polishing liquid
  • SF1 Polishing Fluid
Polishing cloths
  • Chemcloth Polishing Cloths
Rotation
  • Plate
  • Head/Puck
Arm sweep
  • Polishing: 20% (inner) - 100% (outer)
Substrates Sample size
  • one 20x20mm piece
  • one 50 mm wafer
  • one 2" wafer
  • one 100 mm wafer
  • one 150 mm wafer
Allowed materials
  • Silicon
  • Glass/Quartz