Jump to content

Specific Process Knowledge/Etch: Difference between revisions

From LabAdviser
Bghe (talk | contribs)
Bghe (talk | contribs)
Line 62: Line 62:
|-valign="top"
|-valign="top"
|style="background: LightGray"|
|style="background: LightGray"|
*[[/DryEtchProcessing| Dry Etch page: General processing and hardware comparison/manuals]]
*[[/ASE (Advanced Silicon Etch)|ASE (Advanced Silicon Etch)]]
*[[/ASE (Advanced Silicon Etch)|ASE (Advanced Silicon Etch)]]
*[[/AOE (Advanced Oxide Etch)|AOE (Advanced Oxide Etch)]]
*[[/AOE (Advanced Oxide Etch)|AOE (Advanced Oxide Etch)]]
Line 69: Line 70:
*[[/III-V RIE|III-V RIE - Plassys]]
*[[/III-V RIE|III-V RIE - Plassys]]
*[[/IBE⁄IBSD Ionfab 300|IBE/IBSD Ionfab 300]]
*[[/IBE⁄IBSD Ionfab 300|IBE/IBSD Ionfab 300]]
*[[/DryEtchProcessing| Dry Etch page: General processing and hardware comparison/manuals]]
|style="background: #DCDCDC"|
|style="background: #DCDCDC"|
*[[/Wet Silicon Nitride Etch|Wet Silicon Nitride Etch]]
*[[/Wet Silicon Nitride Etch|Wet Silicon Nitride Etch]]

Revision as of 12:03, 12 November 2018

Feedback to this page: click here


Wet etch or dry etch

Etching at Danchip can be done either with wet chemistry or in dry etch equipment. In general wet chemistry etches isotropically in most materials were as dry etch techniques can be optimized to transfer a given mask pattern with vertical sidewalls (anisotropically) to a given substrate.

Advantages of wet chemistry over dry etch techniques are:

  • An often high etch rate difference of different materials giving raise to a high selectivity of the material to be etched compared to underlaying layers or mask materials.
  • Time saving: You can often etch 25 wafers at a time in wet chemistry where as dry etch equipment can only handle one wafer at a time.
  • Easy to start up new etch solutions.

Advantages of dry etch over wet chemistry:

  • Anisotropic etch can be done.
  • The etch does not attack the backside of the sample.

Dry etch Tool Package Training

Choose material to be etched

Dry etching of III-V materials and exotic materials in some other European Cleanroom facility

Dielectrica Semicondutors Metals Alloys Polymers
  • No results, use IBE

Choose Method/Equipment for the Etch

A Dry Etch Equipment A Wet Etch