Line 84: Line 84:
* The Lorentzian-to-Gaussian ratio is freed. Before, it was set to 100.
* The Lorentzian-to-Gaussian ratio is freed. Before, it was set to 100.
* The three asymmetry parameters 'Tail Mix', 'Tail Height' and 'Tail Exponent' are also free to find a minimum within some restricted range on the condition that the parameters of the two peaks be the same.
* The three asymmetry parameters 'Tail Mix', 'Tail Height' and 'Tail Exponent' are also free to find a minimum within some restricted range on the condition that the parameters of the two peaks be the same.
An optimum fit is produced and accepted. In this case the outcome of the fitting is irrelevant for us - the interesting part is the the Peak table. To save it, click the 'Save Peak Table' button shown in the green square and save as *.vgt file.
An optimum fit is produced and accepted. In this case the outcome of the fitting is irrelevant for us - the interesting part is the the Peak table. To save it, click the upper 'Save Peak Table' button shown in the green square and save as *.vgt file. To load the peak table into our Ti2p fitting, click the lower 'Load Peak Table' in the green square.