So far we did not add any constraints at all. That means the Al2p spin orbit doublet is free to shift binding energy or FWHM. | So far we did not add any constraints at all. That means the Al2p spin orbit doublet is free to shift binding energy or FWHM. | ||
[[File:ALD sandwidh Al2p.gif | [[File:ALD sandwidh Al2p.gif]] | ||