= XPS analysis of ALD deposited layers =
= XPS analysis of ALD deposited layers =
This section assumes that you are familiar with the basic operations of data processing in Avantage. If not, then press [[Specific Process Knowledge/Characterization/XPS/Processing/Basics|'''HERE''']] and go through this part first.


This section assumes that you are familiar with the basic operations of data processing in Avantage. If not, then press [[Specific Process Knowledge/Characterization/XPS/Processing/Basics|'''HERE''']] and go through this part first.
== Guidelines on data processing ==
Click [[Specific Process Knowledge/Characterization/XPS/Processing/Guidelines|'''HERE''']] to see some general guidelines on data processing in Avantage.


== How to get the data used in the example below ==
== How to get the data used in the example below ==
Line 8: Line 10:
# Rename the downloaded file Experiment_2.''xls'' to Experiment_2.''zip''
# Rename the downloaded file Experiment_2.''xls'' to Experiment_2.''zip''
# Extract to a folder on a local drive (right click and select 'Extract all'). Avantage will not work on network drives.
# Extract to a folder on a local drive (right click and select 'Extract all'). Avantage will not work on network drives.
# Double click on the ''Experiment 2.VGX'' file and Avantage should start.


== Guidelines on data processing ==


Click [[Specific Process Knowledge/Characterization/XPS/Processing/Guidelines|'''HERE''']] to see some general guidelines on data processing in Avantage.
== Open the experiment ==
 
Double click on the ''Experiment 2.VGX'' file and Avantage should start.
 
[[File:ALD-Sandwich-01.jpg|700px]]

Revision as of 09:53, 16 October 2018

XPS analysis of ALD deposited layers

This section assumes that you are familiar with the basic operations of data processing in Avantage. If not, then press HERE and go through this part first.

Guidelines on data processing

Click HERE to see some general guidelines on data processing in Avantage.

How to get the data used in the example below

The wiki does not allow uploading of *.zip data files so the zipped data file has been renamed to a *.xls file. Therefore, do the following:

  1. Download this File:Experiment 2.xls.
  2. Rename the downloaded file Experiment_2.xls to Experiment_2.zip
  3. Extract to a folder on a local drive (right click and select 'Extract all'). Avantage will not work on network drives.


Open the experiment