== Guidelines on data processing ==
; Use one processing grid to hold all spectra to be fitted.
: Each processing grid has a peak table that holds all the peaks for each level. Making depth profiles cannot be made across processing grids. Survey spectra must be kept in separate grids - if not the peak table of the survey spectrum will get mixed with the high resolution spectra.


; Do not mix snapshot and scanned spectra in processing grid
Click [[Specific Process Knowledge/Characterization/XPS/Processing/Guidelines|'''HERE''']] to see some general guidelines on data processing in Avantage.
: