==Acceptance test and test results==
==Temescal acceptance test results==
[[File:w26 with resist02.jpg|400px|right|thumb|Si wafer with nLOF resist pattern and 10 nm Ti/100 nm Au on top. The side wall is free of deposition]]
[[File:w26 with resist02.jpg|400px|right|thumb|Si wafer with nLOF resist pattern and 10 nm Ti/100 nm Au on top. The side wall is free of deposition]]