| Line 121: | Line 121: | ||
==The E-beam and the Cu hearth== | ==The E-beam and the Cu hearth== | ||
[[File:Cu hearth.jpg| | [[File:Cu hearth.jpg|200px|left|thumb|E-beam impinging on the target from the filament and a 6-pocket Temescal copper hearth and filament box enclosed in its shields (from Scotech)]] | ||
[[File:Cu hearth 2.jpg|100px|right|thumb|Empty 6-pocket Temescal copper heath (from Fil-Tech)]] | [[File:Cu hearth 2.jpg|100px|right|thumb|Empty 6-pocket Temescal copper heath (from Fil-Tech)]] | ||