| Date | Substrate Information | Process Information | SEM Images | |||
|---|---|---|---|---|---|---|
| Wafer info | Exposed area | Conditioning | Recipe | Wafer ID | ||
| 2/5-2016 | 4" Travka20 Wafer | 20 % Si | 3 minute TDESC clean | PrA-0, 80 cycles or 14:40 minutes | C03991.01 | |
| 2/5-2016 | 4" Travka20 Wafer | 20 % Si | 3 minute TDESC clean | PrA-0, 80 cycles or 14:40 minutes | C03991.04 | |
| 3/6-2016 | 4" Travka20 Wafer | 20 % Si | 3 minute TDESC clean | PrA-0, 80 cycles or 14:40 minutes | C04047.01 | |
| 3/6-2016 | 4" Travka20 Wafer | 20 % Si | 3 minute TDESC clean | PrA-0, 80 cycles or 14:40 minutes | C04047.04 | |