s1= s2 = s3 = s, the resistivity is given by:
s1= s2 = s3 = s, the resistivity is given by:


ρ = 2aπsV/I                                         Eq.1
ρ = 2aπsV/I   (1)


where a is the thickness correction factor for thicknesses t equal to or less than half the probe spacing (t/s < 0.5):
where a is the thickness correction factor for thicknesses t equal to or less than half the probe spacing (t/s < 0.5):


a = 0.72t/s    Eq.2
a = 0.72t/s    (2)


Substituting Eq. 2 in Eq. 1 we get:
Substituting Eq. 2 in Eq. 1 we get:


ρ = 2aπsV/I = 4.53V/I    Eq.3
ρ = 2aπsV/I = 4.53V/I    (3)


If both sides of Eq. 3 are divided by t we get:
If both sides of Eq. 3 are divided by t we get: