LabAdviser/314/Microscopy 314-307/SEM/Nova/Micro 4-point probe: Difference between revisions
Appearance
| Line 28: | Line 28: | ||
In this thesis, a variation of the classic 4-point probe method was used, called micro 4-point probe (μ4PP). This because the electrodes of the 4-point probe can easily scratch a metallic film with thickness in the nm range, thus reaching the substrate and giving inaccurate electrical measurements as result. Fig. 2a shows a μ4PP probe chip. Visible are the ceramic substrate, the Ag/Pd connector strips and the Si base from which the four cantilevers extend. For the movements, the probe chip is connected to a micromanipulator inside a SEM. Aided by SEM imaging, the probe gently touches the thin-film surface in 2-point probe mode without scratching it, followed by the collection of the data in 4-point probe mode (Fig. 2b). | In this thesis, a variation of the classic 4-point probe method was used, called micro 4-point probe (μ4PP). This because the electrodes of the 4-point probe can easily scratch a metallic film with thickness in the nm range, thus reaching the substrate and giving inaccurate electrical measurements as result. Fig. 2a shows a μ4PP probe chip. Visible are the ceramic substrate, the Ag/Pd connector strips and the Si base from which the four cantilevers extend. For the movements, the probe chip is connected to a micromanipulator inside a SEM. Aided by SEM imaging, the probe gently touches the thin-film surface in 2-point probe mode without scratching it, followed by the collection of the data in 4-point probe mode (Fig. 2b). | ||
[[File:Picture1.png|400px|center|Figure 2. a) General view of a μ4PP probe chip, with the ceramic substrate, the Ag/Pd connector strips and the Si base connected to the four cantilevers; b) SEM micrograph of the four Au covered SiO2 cantilevers correctly landed on the thin- | [[File:Picture1.png|400px|center|Figure 2. a) General view of a μ4PP probe chip, with the ceramic substrate, the Ag/Pd connector strips and the Si base connected to the four cantilevers; b) SEM micrograph of the four Au covered SiO2 cantilevers correctly landed on the thin-film surface.]] | ||
[[File:Picture2.png|500px|thumb|Fig. 1. Schematic representation of the "thin-film structure-property causality" approach for the fabrication of thin-films. The study of the interaction between thin-films is added as fundamental step in the process.]] | |||
= Kleindiek micromanipulator = | = Kleindiek micromanipulator = | ||