where a is the thickness correction factor for thicknesses t equal to or less than half the probe spacing (t/s < 0.5):
where a is the thickness correction factor for thicknesses t equal to or less than half the probe spacing (t/s < 0.5):
a = 0.72t/s


Substituting Eq. 2.9 in Eq. 2.8 we get:
Substituting Eq. 2.9 in Eq. 2.8 we get: