Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange: Difference between revisions
Appearance
No edit summary |
|||
| Line 4: | Line 4: | ||
= Modification of showerhead in december 2014 = | = Modification of showerhead in december 2014 = | ||
This page describes why the showerhead has been changed and what process changes have been found. | This page describes why the showerhead has been changed and what process changes have been found. SPTS calls this modification the 'High Flow Plenum upgrade'. | ||
== Motivation == | == Motivation == | ||