Deposition of TiW alloy can take place in the Wordentec.


Sputter deposition (Wordentec)
Batch size
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
Pre-clean RF Ar clean
Layer thickness .
Deposition rate Depending on process parameters, see here.


This is done by a sputtering process. Process parameters (argon pressure and effect) can be varied, the surface roughness and the deposition rate (see here) and may change with these settings.