Specific Process Knowledge/Lithography/Aligners/Aligner: Maskless 01 processing: Difference between revisions
Appearance
| Line 26: | Line 26: | ||
==Resolution[[Image:section under construction.jpg|70px]]== | ==Resolution[[Image:section under construction.jpg|70px]]== | ||
The pixel-size of the DMM is 0.5µmX0.5µm (at the sample surface), so this is the ultimate resolution of the Aligner: Maskless 01, and also the smallest step that will produce features of different size. The lithographic resolution of the machine is 1µm on paper, which was demonstrated in the acceptance test after installation | The pixel-size of the DMM is 0.5µmX0.5µm (at the sample surface), so this is the ultimate resolution of the Aligner: Maskless 01, and also the smallest step that will produce features of different size. The lithographic resolution of the machine is 1µm on paper, which was demonstrated in the acceptance test after installation using a resist thickness of 0.5µm. In 1.5µm thick resist, the resolution is around 2µm. | ||
The table below shows | |||
... The effect of serifs is significant below 2µm, but negligible above 4µm. | ... The effect of serifs is significant below 2µm, but negligible above 4µm. | ||