Deposition of Hafnium Oxide
Thin films of hafnium oxide, HfO2, can both be deposited both in the ALD1 and the ALD2 (PEALD). However, it is preferred to use the ALD1, as the ALD2 is mainly dedicated for nitride deposition.
More information about hafnium oxide deposition can be found here: for ALD1 and for ALD2 (PEALD).
Deposition of hafnium oxide
| ALD1 |
| |
|---|---|---|
| Generel description |
| |
| Stoichiometry |
|
|
| Film Thickness |
|
|
| Deposition rate |
|
|
| Step coverage |
|
|
| Process Temperature |
|
|
| Substrate size |
|
|
| Allowed materials |
|
|