Specific Process Knowledge/Etch/KOH Etch/ProcessInfo: Difference between revisions

Kabi (talk | contribs)
No edit summary
Kabi (talk | contribs)
Line 71: Line 71:




<math> \frac{(0.85wt% \cdot X)}{(X+1000g)}=Y</math>
<math> \frac{(0.85 \cdot X)}{(X+1000g)}=Y</math>




<math>X=\frac{(Y\cdot 1000g)}{(0.85wt%-Y)}</math>
<math>X=\frac{(Y\cdot 1000g)}{(0.85-Y)}</math>




Line 82: Line 82:




<math>\frac{(0.5wt%\cdot 1.509g/ml\cdot X)}{(X\cdot 1.509g/ml+1000g)}=Y</math>
<math>\frac{(0.5\cdot 1.509g/ml\cdot X)}{(X\cdot 1.509g/ml+1000g)}=Y</math>