| Line 69: | Line 69: | ||
<math>(0.85 ∙X)/(X+1000g)=Y</math> | <math> (0.85 ∙X)/(X+1000g)=Y</math> | ||
<math>X=(Y∙1000g)/(0.85-Y)</math> | <math> X=(Y∙1000g)/(0.85-Y)</math> | ||
So for a 10wt% solution you will need 133 g pills for each liter of water. | So for a 10wt% solution you will need 133 g pills for each liter of water. | ||