Specific Process Knowledge/Characterization/Hardness measurement: Difference between revisions
Appearance
| Line 17: | Line 17: | ||
|- | |- | ||
| | | | ||
There is no scheduled calibration of this machine. We do however have three calibration samples which can be used to verify proper operation of the machine. The calibration samples are also good for practicing the measurement procedure. Calibration samples are available in the following three hardnesses: 277 HV, 464 HV and 704 HV. They have been calibrated using 1 kgf | There is no scheduled calibration of this machine. We do however have three calibration samples which can be used to verify proper operation of the machine. The calibration samples are also good for practicing the measurement procedure. Calibration samples are available in the following three hardnesses: 277 HV, 464 HV and 704 HV. They have been calibrated using a test force of 1 kgf and an indentation time of 10 sec. | ||
|} | |} | ||