Jump to content

Specific Process Knowledge/Characterization/Hardness measurement: Difference between revisions

Choi (talk | contribs)
Choi (talk | contribs)
Line 17: Line 17:
|-
|-
|  
|  
There is no scheduled calibration of this machine. We do however have three calibration samples which can be used to verify proper operation of the machine. The calibration samples are also good for practicing the measurement procedure. The calibration samples are available in the following three hardnesses: 2xx HV, 4xx HV and 6xx HV.
There is no scheduled calibration of this machine. We do however have three calibration samples which can be used to verify proper operation of the machine. The calibration samples are also good for practicing the measurement procedure. The calibration samples are available in the following three hardnesses: 277 HV, 464 HV and 704 HV.
|}
|}