The measured standard hardnesses are 2xx HV, 4xx HV and 6xx HV. The QC is performed x times a year.
There is no scheduled calibration of this machine. We do however have three calibration samples which can be used to verify proper operation of the machine. The calibration samples are also good for practicing the measurement procedure. The calibration samples are available in the following three hardnesses: 2xx HV, 4xx HV and 6xx HV.
*[http://www.labmanager.danchip.dtu.dk/d4Show.php?id=1831&mach=xxx The QC procedure]<br>
 
|}
|}


==Equipment performance and process related parameters==
==Equipment performance and process related parameters==