Specific Process Knowledge/Characterization/Hardness measurement: Difference between revisions

From LabAdviser
Choi (talk | contribs)
Created page with "'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Cha..."
 
Choi (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Thickness_Measurer click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Hardness_measurement click here]'''  


==Thickness measurer==
==Hardness measurer==
[[Image:Thicknessmeasurer2007.jpg|thumb|300x300px|Thickness Measurer. Positioned in cleanroom D-3]]
[[Image:Thicknessmeasurer2007.jpg|thumb|300x300px|Thickness Measurer. Positioned in cleanroom D-3]]



Revision as of 13:39, 19 January 2018

Feedback to this page: click here

Hardness measurer

Thickness Measurer. Positioned in cleanroom D-3

The purpose is to measure the thickness of wafers, depths of larger grooves or height of larger mesas.

During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.


The user manual, technical information and contact information can be found in LabManager:

Thickness measurer

Quality Control - Recipe Parameters and Limits

Quality Control (QC) for the Thickness measurer

The measured standard thickness is 0.1 mm. The measured result has to be within ± 0.005 mm. The QC is preformed once a year.


Equipment performance and process related parameters

Purpose

Hardness measurer

  • Wafer thickness
  • Depths of larger grooves
  • Heigth of larger mesas

Performance

Thickness resolution

  • < 5 µm

Substrates

Batch size

  • One sample
Substrate materials allowed
  • No restrictions