Specific Process Knowledge/Wafer cleaning/7-up & Piranha: Difference between revisions
Appearance
| Line 3: | Line 3: | ||
==Cleaning of wafers or masks== | ==Cleaning of wafers or masks== | ||
Cleaning of wafers or masks can be done in dedicated baths ("Wafer | Cleaning of wafers or masks can be done in dedicated baths ("Wafer Cleaning" and "Mask Cleaning" respectively). They are both located inside "Wet bench 03: Wafer and mask cleaning" and both contain concentrated sulfuric acid to which a little ammonium persulfate is added before use. This creates very reactive peroxide species that remove organic traces efficiently. Historically this mixture has also been referred to as "7-Up" because it fizzes and bubbles similar to the 7-Up beverage. | ||
Samples not allowed or not compatible with these baths can be cleaned manually in a beaker filled with the so called "Piranha" mixture using one of the acids/bases fume hoods. This mixture consists of concentrated sulfuric acid and hydrogen peroxide forming very aggressive and reactive peroxide species (as in 7-Up) which is very effective at removing organic | Samples not allowed or not compatible with these baths can be cleaned manually in a beaker filled with the so called "Piranha" mixture using one of the acids/bases fume hoods. This mixture consists of concentrated sulfuric acid and hydrogen peroxide forming very aggressive and reactive peroxide species (as in 7-Up) which is very effective at removing organic contaminants and to a certain extent some metal ions. | ||
Always use one of these cleaning procedures after KOH etch or hot phosphoric acid etch (Nitride etch) to remove alkali ions before further processing. 7-up and Piranha | Always use one of these cleaning procedures after KOH etch or hot phosphoric acid etch (Nitride etch) to remove alkali ions before further processing. 7-up and Piranha should only be used '''AFTER''' stripping resist by other means (e.g. plasma ashing or using the "Resist strip" bath). Cleaning samples with resist coatings or significant amounts of other organic substances can be very dangerous, because 7-Up and Piranha are so aggressive. '''These solutions are intended for removing TRACES of organic matter. Adding large amounts of organics can lead to explosive reactions!''' | ||
[[Image:7-up_RR3.jpg|300x300px|right|thumb|'Wafer clean' bath in cleanroom D3]] | [[Image:7-up_RR3.jpg|300x300px|right|thumb|'Wafer clean' bath in cleanroom D3]] | ||