Probe station

Probe station. Positioned in serviceroom CX1

Feedback to this page: click here

The Probe station is a - EPS150Triax - Cascade. The purpose is to measure I/V measurement, ohmic measurements etc. It has 4 individually adjustable triax connected probes, but can be fitted with additional coax connected probes. The stage can be moved in x and y to step and repeat a measurement over a large number of chips.

Samples can be inspected by either a microscope and/or a camera.

Two Keithley 2450 source meters are connected to the probe station by triax cables. An additional Keithley 2410 source meter and a Keithley 2000 multi meter is connected by coax cables. All Keithleys can also be connected with banana wires.

Equipment performance and process related parameters

Purpose

Electrical measurements

  • I/V
  • Resistance
  • Data collection by PC possible

Performance

Pad size

  • 100x100µm or more

Substrates

Batch size

  • One sample
Substrate materials allowed
  • No restrictions



The user manual, technical information and contact information can be found in LabManager:

Probe station