The RCA clean is used for cleaning wafers before taking them into the furnaces and a few other equipments (check the cross contamination sheet). | The RCA clean is used for cleaning wafers before taking them into the furnaces and a few other equipments (check the cross contamination sheet). As mentioned above a crucial part of the RCA cleaning procedure is the oxidation by H<sub>2</sub>O<sub>2</sub> at elevated temperatures. Therefore, the lifetime of RCA1 and RCA2 solutions is limited to about 1 hour after preparation and heating to 70<sup>o</sup>C because H<sub>2</sub>O<sub>2</sub> decomposes at this temperature. | ||
*RCA1 contains: H<sub>2</sub>O, NH<sub>4</sub>OH and H<sub>2</sub>O<sub>2</sub> (5:1:1). It is used for removal of light organics, particles and metals.<br> | *RCA1 contains: H<sub>2</sub>O, NH<sub>4</sub>OH and H<sub>2</sub>O<sub>2</sub> (5:1:1). It is used for removal of light organics, particles and metals.<br> | ||