The top and bottom heaters of the VPO module are typically set to 120°C. The wafer is baked under a low vacuum (~0.35 bar) in order to heat and dehydrate the wafer before HMDS application. The HMDS is injected into the process chamber using nitrogen as a carrier gas. 10 liters per minute of dry nitrogen is bubbled through liquid HMDS before flowing into the chamber. The injection lasts until ambient pressuer is reached in the chamber. After the reaction time, the chamber is pump-purged using nitrogen. Finally, the wafer is cooled on the cool plate.
The top and bottom heaters of the VPO module are typically set to 120°C. The wafer is baked under a low vacuum (~0.35 bar) in order to heat and dehydrate the wafer before HMDS application. The HMDS is injected into the process chamber using nitrogen as a carrier gas. 10 liters per minute of dry nitrogen is bubbled through liquid HMDS before flowing into the chamber. The injection lasts until ambient pressuer is reached in the chamber. After the reaction time, the chamber is purged using nitrogen. Finally, the wafer is cooled on the cool plate.


The contact angle after HMDS priming is a function of the priming temperature, the priming time, and the surface condition of the wafer. The condition of the substrate surface is again a function of the substrate type, the substrate history, and the effectiveness of the dehydration step. Since the vapor pressure of water at the chamber temperature is much higher than the dehydration pressure, similarly the boiling point of water at the dehydration pressure is well below the chamber temperature, the dehydration can probably be considered to be quite effective. However, for thick oxides, transport effects may cause the 30s dehydration time to be insufficient to dehydrate the surface sufficiently.
The contact angle after HMDS priming is a function of the priming temperature, the priming time, and the surface condition of the wafer. The condition of the substrate surface is again a function of the substrate type, the substrate history, and the effectiveness of the dehydration step. Since the vapor pressure of water at the chamber temperature is much higher than the dehydration pressure, similarly the boiling point of water at the dehydration pressure is well below the chamber temperature, the dehydration can probably be considered to be quite effective. However, for thick oxides, transport effects may cause the 30s dehydration time to be insufficient to dehydrate the surface sufficiently.