Revision as of 08:28, 10 July 2017
Feedback to this page: click here
Choose equipment
Choose bonding methods in Wafer Bonder 2
Comparing the three bonding methods in the wafer bonder 2
| Eutectic bonding | Fusion bonding | Anodic bonding | |
|---|---|---|---|
| General description | For bonding two substrates by use of an interphase that makes an eutecticum. | For bonding two identical materials. | For bonding Si and Glass. |
| Bonding temperature | Depending on the eutecticum 310°C to 400°C. | Depending on defects 50°C to 400°C. | Depending on the voltage 300°C to 500°C Standard is 400°C. |
| Annealing temperature | No annealing | 1000°C-1100°C in the anneal bond furnace (C3). | No annealing |
| Materials possible to bond | Bonding of substrates is done by use of the eutectica Au/Si, Au/Sn and Au/Sn/Ni | Si/Si, SiO2/SiO2 | Si/Pyrex (glass) |
| Substrate size | Up to 4" | Up to 4" | Up to 4" |
| Cleaning | Cleaning by N2. | Wet chemical cleaning, IMEC. | Cleaning by N2. |
| Backside alignment | Double side polished wafers. | Double side polished wafers. | Not relevant. |