== Parameters ==
== Parameters ==
<!-- revised 1/6-2015 by jmli -->
<!-- revised 1/6-2015 by jmli -->

Revision as of 11:45, 27 June 2017

Parameters

Solid shade
In the image the following parameters are shown:
  • Top Width (TW)
  • Depth (D)
  • Bottom Width (BW)
  • Mid Width (MW)

To speed up the characterisation post-SEM the parameter 'Pixel Size' (PS) is added to the SEM databar (the blue circle).

Depth D*PS
Bowing 2MW−TW+BW2(TW+BW)
Sidewall angle acos(TW−BW2D2+14(TW2−BW2))