The following links give an approximate oxide time/thickness based on prediction equations from the following experiments: | The following links give an approximate oxide time/thickness based on prediction equations from the following experiments: | ||
[[media:Calculation_for_Wet_oxidation_for_Anneal_Oxide(C1)_version_2.xlsx|'''Calculation for wet oxidation''']] updated on June 2017 | [[media:Calculation_for_Wet_oxidation_for_Anneal_Oxide(C1)_version_2.xlsx|'''Calculation for wet oxidation''']] ''updated on June 2017'' | ||
==Test of the wet oxidation by steamer== | ==Test of the wet oxidation by steamer== | ||