The MVD coatings are created as self-assembled monolayers on a surface when a molecular vapor of chemials is present.  
The MVD coatings are created as self-assembled monolayers on a surface when a molecular vapor of chemials is present.  


These chemicals, typically it is flourinated organosilanes, have a teflon-like tail consisting of -(CF<sub>2</sub>)<sub>x</sub>CF<sub>3</sub> and, in the other end, a reactive group -SiCl<sub>x</sub>. The chlorine atoms react with -OH groups of the surface to form a chemical bond under elimination of HCL.  
These chemicals, typically it is flourinated organosilanes, have a teflon-like tail consisting of -(CF<sub>2</sub>)<sub>x</sub>CF<sub>3</sub> and, in the other end, a reactive group -SiCl<sub>x</sub>. As shown in the figure below, the chlorine atoms react with -OH groups of the surface to form a chemical bond under elimination of HCL. This means that both Si and SiO<sub>2</sub> surfaces are coated.
 
 