==Sputtering of Nickel Vanadium== | ==Sputtering of Nickel Vanadium== | ||
Nickel Vanadium may be sputter deposited in either Sputter-system (Lesker) | Nickel Vanadium may be sputter deposited in either Sputter-system (Lesker) or Wordentec | ||
* [[/Sputtering of NiV in Lesker|Sputtering of NiV in Lesker]] | |||
* [[/Sputtering of NiV in Wordentec|Sputtering of NiV in Wordentec]] | * [[/Sputtering of NiV in Wordentec|Sputtering of NiV in Wordentec]] | ||
In the chart below you can compare the different deposition equipment. | In the chart below you can compare the different deposition equipment. | ||
Revision as of 13:37, 2 January 2017
Feedback to this page: click here
Sputtering of Nickel Vanadium
Nickel Vanadium may be sputter deposited in either Sputter-system (Lesker) or Wordentec
In the chart below you can compare the different deposition equipment.
| Sputter deposition (Sputter-System Lesker) | Sputter deposition (Wordentec) | |
| General description | Sputter deposition of NiV | Sputter deposition of NiV |
| Pre-clean | RF Ar clean | RF Ar clean |
| Layer thickness | About 10Å to 5000Å | |
| Deposition rate | Depending on process parameters. | Depending on process parameters. |
| Batch size |
|
|
| Allowed substrates |
|
|
| Allowed materials |
|
|
| Comment | Sputter target with NiV composition: Ni/V 93/7% | Sputter target with NiV composition: Ni/V 93/7% |