At Danchip, we have two types of bulk glass substrates: Borosilicate glass (Borofloat 33 (like pyrex)) and fused silica glass which in cleanliness is similar to quartz. Both types are etched wet in a special set-up placed in a fumehood using a strong HF-solution (isotropic etch).
At Danchip, we have two types of bulk glass substrates: Borosilicate glass (Borofloat 33 (like pyrex)) and fused silica glass which in cleanliness is similar to quartz. Both types are etched wet in a special set-up placed in a fumehood using a strong HF-solution (isotropic etch).
The set-up consists of a 5 l plasic beaker placed on a stirring plate (magnetic stirring) and a special horizontal wafer holder. Normally a 40% pre-mixed HF solution is used.
The set-up consists of a 5L plasic beaker placed on a stirring plate (magnetic stirring) and a special horizontal wafer holder. Normally a 40% pre-mixed HF solution is used.


Masking materials and pre-treatment of the glass surface prior to the deposition of the masking material is a special concern in particular for deep etchings (> 10µm).   
Masking materials and pre-treatment of the glass surface prior to the deposition of the masking material is a special concern in particular for deep etchings (> 10µm).   
Line 6: Line 6:
Due to the high cleanliness fused silica is allowed access to basically all machines meaning that e.g. LPCVD silicon can be deposited as masking material. This is an excellent mask even for quite deep etchings.
Due to the high cleanliness fused silica is allowed access to basically all machines meaning that e.g. LPCVD silicon can be deposited as masking material. This is an excellent mask even for quite deep etchings.


Regarding borosilicate glass masking is more tricky. The follwing sequence has been used with some success (using sputtered silicon from the Alcatel):
Regarding borosilicate glass masking is more tricky. The following sequence has been used with some success (using sputtered silicon from the Alcatel):


* Piranha clean
* Piranha clean