| Line 72: | Line 72: | ||
There are no standard injection moulding processes because it varies significantly how users prefer to optimize their process and how they prioritize parameters such as polymer type, replication fidelity, dimensional accuracy, optical properties, residual stress and cycle time. However, browsing through the [http://labmanager.dtu.dk/function.php?module=Processlog&view=editlog&machid=278 Process Log] it's usually not a problem to find a program made for the polymer and tool at hand which can be used as a starting point. | There are no standard injection moulding processes because it varies significantly how users prefer to optimize their process and how they prioritize parameters such as polymer type, replication fidelity, dimensional accuracy, optical properties, residual stress and cycle time. However, browsing through the [http://labmanager.dtu.dk/function.php?module=Processlog&view=editlog&machid=278 Process Log] it's usually not a problem to find a program made for the polymer and tool at hand which can be used as a starting point. | ||
The injection moulding cycle consists of the steps outlined below. Click on each step to get a description of the most important process parameters for each step: | |||
===[[Specific Process Knowledge/Back-end processing/Polymer Injection Molder/Mold temperature setup]=== | |||
===[[Specific Process Knowledge/Back-end processing/Polymer Injection Molder/Closing mold]=== | |||
===[[Specific Process Knowledge/Back-end processing/Polymer Injection Molder/Injection]=== | |||
===[[Specific Process Knowledge/Back-end processing/Polymer Injection Molder/Switch-over type]=== | |||
===[[Specific Process Knowledge/Back-end processing/Polymer Injection Molder/After (holding) pressure]=== | |||
===[[Specific Process Knowledge/Back-end processing/Polymer Injection Molder/Cooling]=== | |||
===[[Specific Process Knowledge/Back-end processing/Polymer Injection Molder/Dosing (plasticising)]=== | |||
===[[Specific Process Knowledge/Back-end processing/Polymer Injection Molder/Demoulding]=== | |||
===[[Specific Process Knowledge/Back-end processing/Polymer Injection Molder/Ejection and robot pickup]=== | |||