*PMMA<br>
*PMMA<br>


Topas polymers are supplied by Danchip. All other polymers are purchased by the users themselves. All polymers must be approved for use at DTU Danchip. If you would like to use a new polymer or a new grade of a certain polymer, please fill out the New_polymer_application.dotx form which can be found in LabManager by going to the Documents tab of the 'Info' page for the Polymer Injection Molding machine. You can also use this direct link: [http://labmanager.dtu.dk/view_binary.php?fileId=2857 New_polymer_application]
Topas polymers are supplied by Danchip. All other polymers are purchased by the users themselves. All polymers (and each individual grade of each polymer) must be approved for use at DTU Danchip. If you would like to use a new polymer or a new grade of a certain polymer, please fill out the '''''New_polymer_application.dotx''''' form which can be found in LabManager by going to the 'Documents' tab of the 'Info' page for the Polymer Injection Molding machine. You can also use this direct link: [http://labmanager.dtu.dk/view_binary.php?fileId=2857 New_polymer_application.dotx]


When the polymer has been approved you will receive some labels which must be used to label your polymer. All polymers left in the injection moulding room must be marked with this official Danchip label. Polymers not labelled appropriately may be thrown out at any time.
When the polymer has been approved you will receive labels which must be used to label your polymer. All polymers left in the injection moulding room must be marked with this official DTU Danchip label. '''Polymers not labelled appropriately may be thrown out at any time'''.


The easiest way to get an overview of polymers and processes used on the polymer injection moulding machine is to go to LabManager and consult the [http://labmanager.dtu.dk/function.php?module=Processlog&view=editlog&machid=278 Process Log] for the injection moulding machine. Please remember that all polymers besides Topas and PS 158K (polystyrene) are property of individual users and only approved for use by specific user.
The easiest way to get an overview of polymers and processes used on the polymer injection moulding machine is to go to LabManager and consult the [http://labmanager.dtu.dk/function.php?module=Processlog&view=editlog&machid=278 Process Log for the injection moulding machine]. If you would like use a non-Danchip polymer for a test, please contact the owner of the polymer and ask if you can have a sample. A complete list of all polymers in use at DTU Danchip and who owns them can be found here:
 
If you would like use a non-Danchip polymer for a test, please contact the owner of the polymer and ask if you can have a sample.


==Equipment performance==
==Equipment performance==